MTI | SKU:
bcnf-16m2
Nickel Foam (200mm length x 300mm width x 1.6mm thickness) - EQ-bcnf-16m-2
€60,88
Unit price
/
Unavailable
Couldn't load pickup availability
Delivery and Shipping to EU
Delivery and Shipping to EU
We will add in the quotation, the shipping, insurance, customs clearance costs.
Nickel Foam (200mm length x 300mm width x 1.6mm thickness) - EQ-bcnf-16m-2
MTI
Specifications
- Material: Nickel Foam, Purity> 99.99% (excellent anti-corrosive)
-
Sold in roll onlySurface Density: 346g/m^2
- Length: 200 mm
- Width: 300mm
- Thickness: 1.6 mm
- Net weight: 21g
- Porosity: ?95% (80-110 Pores per Inch. average hole diameters about 0.25mm)
- Extensibility: Lengthwise?5%; Widthwise?12%
- Tensile StrengthLengthwise?1.25N/mm^2; Widthwise?1.00N/mm^2
- Notice: Please notice that it is normal to observe NiO peaks in the nickel foam in XRD data. It is really difficult to avoid the oxidation of the nickel.
- How to clean the Nickel Foam for Battery Cathode Substrate.
- It can be removed the NiO by annealing in the hydrogen furnace.
- Nickel foam (about 3.3 cm x 1 cm) was carefully cleaned with the concentrated HCl solution (37 wt.%) in an ultrasound bath for 5 min in order to remove the surface oxide layer. And then deionized water and absolute ethanol were used for 5 min each to ensure the surface of the Ni foam was well cleaned.
![]() ![]() Porosity: ?95% (80-110 Pores per Inch, average hole diameter is about 0.25mm |
![]() Click the video above to see the battery cathode coated by MTI's Film coater MSK-AFA-II-VC |
![]() Other Metallic Foams |
Related Product
![]() Battery Powders |
![]() Heatable Ultrasonic Cleaner |
![]() Electrode Coating |
![]() Coin Cell Assembling |
![]() Pouch Cell Assembling |
![]() Cylinder Cell Assembling |
![]() Electrolyte injection |
![]() New innovation in MTI |