5 mm Thick Nickel Foam (L 200mm L x W 300mm) - bcnf-5
MTI
Specifications
- Material: Nickel Foam, Purity> 99.99% (excellent anti-corrosive)
-
Sold in one pieceSurface Density: 800g/m^2
- Length: 200 mm
- Width: 300mm
- Thickness: 5mm
- Porosity: ?95% (80-110 Pores per Inch. average hole diameters about 0.25mm)
- Extensibility: Lengthwise?5%; Widthwise?12%
- Tensile StrengthLengthwise?1.25N/mm^2; Widthwise?1.00N/mm^2
- Notice: Please notice that it is normal to observe NiO peaks in the nickel foam in XRD data. It is really difficult to avoid the oxidation of the nickel.
- How to clean the Nickel Foam for Battery Cathode Substrate.
- It can be removed the NiO by annealing in the hydrogen furnace.
- Nickel foam (about 3.3 cm x 1 cm) was carefully cleaned with the concentrated HCl solution (37 wt.%) in an ultrasound bath for 5 min in order to remove the surface oxide layer. And then deionized water and absolute ethanol were used for 5 min each to ensure the surface of the Ni foam was well cleaned.
![]() ![]() Porosity: ?95% (80-110 Pores per Inch, average hole diameter is about 0.25mm |
![]() Click the video above to see the battery cathode coated by MTI's Film coater MSK-AFA-II-VC |
![]() Other Metallic Foams |
Related Product
![]() Battery Powders |
![]() Heatable Ultrasonic Cleaner |
![]() Electrode Coating |
![]() Coin Cell Assembling |
![]() Pouch Cell Assembling |
![]() Cylinder Cell Assembling |
![]() Electrolyte injection |
![]() New innovation in MTI |