Conductive Acetylene Black for Li-ion Battery Anode/Cathode, 50 g/bag - EQ-Lib-AB
Couldn't load pickup availability
Delivery and Shipping to EU
Delivery and Shipping to EU
We will add in the quotation, the shipping, insurance, customs clearance costs.
Conductive Acetylene Black for Li-ion Battery Anode/Cathode, 50 g/bag - EQ-Lib-AB
MTI
- Cathode: Cathode Active+Acetylene Black (Conductive)+PVDF+NMP
- Anode: Anode Active+Acetylene Black (Conductive)+PVDF+NMP (or SBR+CMC)

Apparent Specific Volume |
16~17 ml/g |
Iodine Absorption Number |
?90 g/kg |
Hydrochloric Acid Absorption Number |
?4.4 ml/g |
Resistivity |
?1.8 ?/m |
PH Value |
6~8 |
Heating Loss |
?0.2% |
Ash Content |
?0.2% |
Grid Content (sieve with 325 grid) |
?0.003% |
Particle Size |
35~40 nm |
Impurity |
None |
Absorption Intensity |
?23.4 ml/5g |
Oil-Absorption |
?250 ml/100g |
Package | Container Sealed in Al Vacuumed Bag |
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in a vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity
![]() Vacuum Storage Box |
![]() Powder Milling & Mixer |
![]() Electrode Coaters |
![]() Battery Research Equipment |
![]() Other Battery Powder |